GH333 Alloy: Nickel-based superalloy with high strength, excellent oxidation resistance, and thermal stability

Jiangsu Zhonggongte Metallurgical Technology Co., Ltd.
Contact Now

GH333 Alloy: Nickel-based superalloy with high strength, excellent oxidation resistance, and thermal stability

  • 1
  • 2

Brand Name : Zhonggong Special Metallurgy

Model Number : GH333 Alloy

Place of Origin : China

MOQ : 100KG

Price : Price is negotiated based on the required specifications and quantity

Payment Terms : Payment Terms: Mainly T/T.. L/C, D/A, D/P,

Supply Ability : 5000 tons per month

Delivery Time : 5-8 working days, depending on the parameters required for negotiation

Packaging Details : Standard export packaging, or packaging as required

Material Type : Nickel-based Superalloy

Density : ~8.3 g/cm³

Tensile Strength : ~850 MPa

Yield Strength : ~700 MPa

Temperature Range : Up to 950°C (1742°F)

Oxidation Resistance : Excellent

Corrosion Resistance : Good

Applications : Aerospace, power generation, chemical processing

Heat Treatment : Solution treated and aged

Certification : ISO Certificate

Contact Now

GH333 Alloy is a high-performance nickel-based superalloy engineered for demanding high-temperature applications. It is designed to deliver exceptional strength, durability, and resistance to harsh environments, making it suitable for critical components in aerospace and industrial sectors.

Key Features:

  • Composition: Primarily nickel with chromium, molybdenum, titanium, and aluminum, tailored to enhance its mechanical properties and resistance to heat.
  • Temperature Resistance: Effective in environments up to 950°C (1742°F), where it maintains structural integrity and performance.
  • Mechanical Properties: Provides high tensile and yield strength, ensuring reliability and stability under extreme stress conditions.
  • Oxidation and Corrosion Resistance: Excellent resistance to oxidation and corrosion, extending the lifespan of components in aggressive environments.
  • Applications: Ideal for use in aerospace engine components, industrial gas turbines, exhaust systems, and chemical processing equipment, where high-temperature stability and durability are crucial.
  • Heat Treatment: Capable of being heat-treated to achieve optimal mechanical properties, including improved strength and toughness, offering flexibility in manufacturing processes.

GH333 Alloy’s advanced properties make it an ideal choice for applications requiring high performance, resistance to extreme temperatures, and reliable long-term operation. Its robust nature ensures dependable service in some of the most challenging industrial and aerospace environments.


Product Tags:

high strength nickel based alloys

      

high strength nickel based superalloy

      
Quality GH333 Alloy: Nickel-based superalloy with high strength, excellent oxidation resistance, and thermal stability for sale

GH333 Alloy: Nickel-based superalloy with high strength, excellent oxidation resistance, and thermal stability Images

Inquiry Cart 0
Send your message to this supplier
 
*From:
*To: Jiangsu Zhonggongte Metallurgical Technology Co., Ltd.
*Subject:
*Message:
Characters Remaining: (0/3000)